Figure 3.

Figure 3

Scanning electron microscope of studied ceramics after 48 h. (a) Tetragonal zirconia, (b) Cubic zirconia, (c) Lithium disilicate, (d) Zirconia-reinforced lithium silicate, (e) Hybrid ceramic.