Table 2.

Table of data for tensile stress–strain tests of as-cast Al-Mg-Ga-Sn-In soluble aluminum alloys with different Mg contents at room temperature.

Sample Number σb/MPa σs/MPa δ/% φ/%
ZM0 53.916 ± 0.85 13.866 ± 0.50 10.06 ± 0.90 4.72 ± 1.10
ZM1 94.357 ± 1.30 16.863 ± 0.90 12.17 ± 0.50 5.89 ± 0.50
ZM2 117.883 ± 1.30 17.319 ± 1.00 20.77 ± 0.30 7.84 ± 0.50
ZM3 181.989 ± 1.60 18.541 ± 0.80 27.49 ± 0.30 11.67 ± 0.50
ZM4 154.383 ± 1.30 18.051 ± 1.00 24.31 ± 0.50 8.92 ± 0.50
ZM5 105.078 ± 1.20 12.267 ± 0.80 11.63 ± 0.70 6.42 ± 0.90

The room-temperature compressive stress–strain curves of cast Al-Mg-Ga-Sn-In soluble aluminum alloys with different Mg contents are shown in Figure 11, and the compressive stress–strain test data are shown in Table 3.