Fig. 2.

Fig. 2

(a) The optical microscope (OM) image of the top view of CVD-grown WSe2 with different thicknesses. The scale bar is 10 μm. (b) The comparison of Raman spectra of WSe2 with different thicknesses. The fingerprint of Raman peaks is very sensitive to WSe2 thickness. The inset shows WSe2 Raman spectra focusing on Raman shift from 290 to 320 cm−1.