Skip to main content
. 2024 Nov 20;7:1540. doi: 10.1038/s42003-024-07196-0

Fig. 5. Morphological characterization and surface element analysis of PLGA microspheres.

Fig. 5

A After optimization, with all other conditions held constant, naked-eye images of microspheres were taken when using 200 mg, 100 mg, and 50 mg of PLGA as input material. B Electron microscope images were captured at magnifications of 100×, 300×, 1000×, and 6000×. C Surface element analysis was conducted on microspheres prepared using 100 mg of PLGA, as scanned under an electron microscope.