Skip to main content
. 2024 Nov 20;14:28764. doi: 10.1038/s41598-024-80149-z

Fig. 14.

Fig. 14

Mechanical behavior of SCC and RFC with 10 mm aperture and 10% porosity (a) Stress-strain curve and single-step AE energy (b) AE distribution.