Skip to main content
. 2024 Nov 11;40(46):24516–24527. doi: 10.1021/acs.langmuir.4c03302

Table 2. Detailed Components of Polymers Used in Coating Mixtures.

sample name coating solution formula
Mix 1 3 mL of MPS–PEGMACOOH2.5 + 3 mL of MPS–MPC2.5 (molar fraction: 5:5)
Mix 2 3 mL of MPS–PEGMACOOH2.5 + 3 mL of MPS–MPC2.5 (molar fraction: 7:3)
Mix 3 3 mL of MPS–PEGMACOOH5 + 3 mL of MPS–MPC2.5 (molar fraction: 5:5)