Table 3.
Comparison of contact resistance between theoretical model and experimental results for different loads and numbers of cycles.
Number of Cycles | 2-Times Load | 4-Times Load | 6-Times Load | ||||||
---|---|---|---|---|---|---|---|---|---|
Theoretical Model (mΩ) | Experiment (mΩ) | Error (%) |
Theoretical Model (mΩ) | Experiment (mΩ) | Error (%) |
Theoretical Model (mΩ) | Experiment (mΩ) | Error (%) |
|
0 | 15.52 | 20.55 | −24.48 | 14.59 | 21.06 | −30.72 | 19.95 | 20.49 | −2.64 |
20 | 22.44 | 22.24 | 0.90 | 25.55 | 24.55 | 4.07 | 28.01 | 27.11 | 3.32 |
40 | 27.40 | 25.37 | 8.00 | 31.67 | 29.82 | 6.20 | 33.87 | 34.76 | −2.56 |
60 | 31.39 | 29.16 | 7.65 | 36.35 | 36.47 | −0.33 | 38.76 | 41.5 | −6.60 |
80 | 34.78 | 32.82 | 5.97 | 40.26 | 41.65 | −3.34 | 43.03 | 45.45 | −5.32 |