. 2024 Nov 18;17(22):5622. doi: 10.3390/ma17225622

Table 2.

Results of Vickers microhardness indentation on MS-ZnS, annealed, and of Samples #1, #2, and #3. The data represent the average value (Hv) and standard deviation (σHv) for 100 tests on each sample.

Ga (at. %) Hv (GPa) σHv (GPa)
0 (untreated) 1.77 0.10
0 (annealed) 1.92 0.11
1.8 3.47 0.08
3.0 3.49 0.08
3.6 3.80 0.14