Cementation strength of different ratios of cemented filling slurry at different ages.

Concentration Ratio Age Fitting Result Correlation
71% 5:5 3 y=42.5×0.722×0.066×ex1×x21.19 0.76
71% 5:5 7 y=42.5×0.722×0.77×ex1×x22.78 0.92
71% 5:5 28 y=42.5×0.722×0.731×ex1×x22.40 0.98
71% 4:6 3 y=42.5×0.701×0.055×ex1×x21.1 0.77
71% 4:6 7 y=42.5×0.701×0.58×ex1×x22.56 0.95
71% 4:6 28 y=42.5×0.701×0.56×ex1×x22.22 0.98
71% 3:7 3 y=42.5×0.698×0.053×ex1×x21.21 0.78
71% 3:7 7 y=42.5×0.698×0.7×ex1×x22.9 0.88
71% 3:7 28 y=42.5×0.698×0.51×ex1×x22.32 0.98

Notes: ratio: the weight ratio of yellow phosphorus slag to tailings.