. 2024 Nov 20;17(22):5675. doi: 10.3390/ma17225675

Table 4.

Comparison of von Mises stress (MPa) for EPDM and LSR across different aging conditions using Mooney–Rivlin, Ogden, and Yeoh models.

Location EPDM LSR
Mooney–Rivlin Ogden Yeoh Mooney–Rivlin Ogden Yeoh
No Aging
1st Anode 4.71 24.54 2.04 7.93 73.46 16.11
1st Cathode Up 14.96 78.40 7.26 24.17 245.18 49.64
1st Cathode Down 15.59 77.12 7.19 24.68 229.84 48.83
Heat
1st Anode 4.74 24.41 1.89 7.98 82.61 13.92
1st Cathode Up 15.18 76.30 5.82 24.37 277.51 43.22
1st Cathode Down 15.64 75.30 6.58 24.61 260.11 39.23
Heat + Sulfuric Acid
1st Anode 5.19 5.04 2.33 1.74 1.55 1.50
1st Cathode Up 16.25 16.68 8.42 6.16 5.50 5.41
1st Cathode Down 16.52 17.03 8.51 6.10 5.58 5.34