Skip to main content
. 2024 Nov 20;17(22):5675. doi: 10.3390/ma17225675

Table 5.

Comparison of contact stress (MPa) for EPDM and LSR across different aging conditions using Mooney–Rivlin, Ogden, and Yeoh models.

Location EPDM LSR
Mooney–Rivlin Ogden Yeoh Mooney–Rivlin Ogden Yeoh
No Aging
1st Anode 20.99 75.38 10.81 31.11 211.01 51.35
1st Cathode Up 23.86 91.07 11.46 37.57 261.49 62.93
1st Cathode Down 22.26 85.31 10.98 33.45 277.17 57.61
Heat
1st Anode 21.29 73.32 10.09 31.72 241.29 47.03
1st Cathode Up 24.02 89.09 10.86 38.20 285.88 58.21
1st Cathode Down 22.53 81.14 10.31 33.66 296.93 50.69
Heat + Sulfuric Acid
1st Anode 22.32 20.57 11.75 9.21 8.31 8.10
1st Cathode Up 25.83 23.61 12.76 9.75 8.76 8.50
1st Cathode Down 23.07 21.70 11.90 9.22 8.25 8.18