Skip to main content
. 2024 Oct 11;36(48):2410655. doi: 10.1002/adma.202410655

Figure 4.

Figure 4

Gigantic, isotropic negative MR in GdPS. a) Temperature dependence for in‐plane resistivity ρxx , measured under various magnetic field from 0 to 9 T. Inset: measurement setup. b) Magnetic field dependence for ρxx , measured at various temperatures from 2 to 300 K. c) Angular dependence for MR at T = 5 K for in‐plane resistivity ρxx , measured by rotating field perpendicular to (θ‐dependence, left) and within (φ‐dependence, right) the phosphorus plane. Inset: schematic of magnetic field rotation. d) Temperature dependence for out‐of‐plane resistivity ρzz , measured under various magnetic field from 0 to 9 T. Inset: measurement setup. e) Magnetic field dependence of ρzz , measured at various temperatures from 2 to 300 K. f) Angular dependence for MR at T = 5 K for out‐of‐plane resistivity ρzz , measured by rotating field perpendicular to (θ‐dependence, left) and within (φ‐dependence, right) the phosphorus plane. Inset: schematic of magnetic field rotation.