. 2024 Dec 5;44:572–588. doi: 10.1016/j.bioactmat.2024.10.030

Fig. 2.

Fig. 2

In vitro degradation behavior of Zn and Zn/Ti composites: (a) 3D SVET maps, (b) PDP curves, (c) Bode plots, (d) Overview pictures, SEM and EDS scan images of the sample surface and cross section after 28 days of immersion, (e) XRD patterns of degraded Zn and Zn/Ti samples after 28 days, (f) Corrosion rates, and (g) Zn2+ concentration in HBSS.