Table 2.

Comparisons of loss of tension due to relaxation at 1200 s in Figure 3.

p-Value
Stainless Steel (d = 1.6 mm) vs. Stainless Steel (d = 2.0 mm) 0.2496
Stainless Steel (d = 1.6 mm) vs. Vitallium (d = 1.6 mm) 0.2776
Stainless Steel (d = 1.6 mm) vs. Vitallium (d = 2.0 mm) 0.1551
Stainless Steel (2.0 mm) vs. Vitallium (d = 1.6 mm) 0.8562
Stainless Steel (2.0 mm) vs. Vitallium (d = 2.0 mm) 0.5051
Vitallium (d = 1.6 mm) vs. Vitallium (d = 2.0 mm) 0.3974