Nanoparticle Irradiation Source, Wavelength, and Power Exposure Time Size (nm) Shape Ref.
AgNPs UV-LED (365 nm) 15 min 30 Spherical [229]
AgNPs UV Light 0.362 mW/cm2 3 h 60, 100 Nano prisms, Pentagons [230]
AgNPs UV reactor (UV-A, 6 W) 24 h 19 [231]
AgNPs UV light (λ = 365 nm) 10 min 11.7 ± 7.2 Cubes, rods, and spheres [232]
AgNPs 30 W UV-C bactericidal lamp 45 min 50 Spherical [233]
Ag/Au/AgCl UVC light 4.26 mW/cm2 50 min 96 Nanorod, Spherical [234]
ZnO/Ag UVC light with a wavelength of 254 nm 30 min 100 Hexagonal nanorods [235]
AgNPs Ultraviolet–visible light (EXFO Acticure A4000, 85 mW/cm2) 1 h 3.3 ± 0.7 Spherical [236]