Skip to main content
. 2025 Jan 9;15:1432. doi: 10.1038/s41598-024-83634-7

Table 7.

Result obtain from the experimental of pGFRP cross-arm.

Cross-arm member Location Stress, (MPa) ε0, (10− 4) Inline graphic (GPa)
pGFRP Balau wood pGFRP Balau wood
Main 1 Y1 97.29 3.1731 4.8295 306.62 201.45
Y2 196.04 4.9722 7.8653 394.28 249.25
Y3 294.79 6.7140 8.6914 439.07 339.17
Y4 393.54 5.5815 8.4476 705.08 465.86
Y5 492.29 3.5540 5.9756 1385.21 823.83
Main 2 Y1 97.292 3.2756 4.8295 297.2 201.45
Y2 196.04 5.0479 7.5522 388.41 259.58
Y3 294.79 6.8081 8.6914 433.00 339.17
Y4 393.54 4.0478 8.1082 972.23 485.36
Y5 492.29 3.0664 5.4252 1605.42 907.41