. 2024 Dec 11;16(24):3465. doi: 10.3390/polym16243465

Figure 9.

Figure 9

Figure 9

DSC comparison of Arkema 6002 (red) with MCO-derived 60/40 T/I PEKK (blue) for first (A) and second (B) consecutive heating cycles to 350 °C at a rate of 5 °C/min, demonstrating a similarity in glass transitions.