Table 3.
System | H [GPa] |
Method | Refs. |
---|---|---|---|
Ti-Zr-Mo-C | 24–34 | Coatings (DC magnetron) | This work |
Ti-Nb-C | 20–25 | Bulk (hot press) | Fides et al. [76] |
Ti-Nb-C | 26–29 | Coatings (laser cladding) | Sun et al. [77] |
Ti-Mo-C | 8–10 | Coatings (RF magnetron) | Koutzaki et al. [7] |
Ti-W-C | 15–26 | Coatings (RF magnetron) | Koutzaki et al. [7] |
Ti-Zr-C | 26–33 | Coatings (DC magnetron) | Pogrebnjak et al. [70] |
Ti-Zr-C | 14–34 | Coatings (DC magnetron) | Rodríguez-Hernández et al. [78] |