Table 4. Urbach and energy bandgap values for as-deposited CdS.

Sample Film thickness (nm) Urbach energy (meV) Bandgap (eV)
CdS-0 92.30 174.83 2.44
CdS-1 96.02 168.07 2.44
CdS-2 100.51 115.88 2.45
CdS-3 89.32 331.13 2.45