. 2025 Mar 24;10(12):12214–12223. doi: 10.1021/acsomega.4c10592

Figure 2.

Figure 2

(a–c) Optical microscope and phase images of eyeglass frames produced with the ABS filament at 0.20 mm layer thickness and 230 °C; (d–f) images of frames produced with the PETG filament at the same settings.