Skip to main content
. 2025 Apr 1;16(18):7794–7810. doi: 10.1039/d4sc08595g

Fig. 3. XRD patterns for BiVO4 films grown on FTO-coated glass by AACVD before annealing (as deposited) and after annealing at 500 °C for 2 hours in air. Data is plot alongside PDF card references patterns for SnO2 (i.e. the FTO substrate), BiVO4, Bi2VO5, Bi2O3 and V2O5.