Table 11. Comparison of corrosion inhibitor performance with other polymers.
| Compound | Inhibition efficiency | Concentration and medium | Ref |
|---|---|---|---|
| (p-Semidine-guanidine-formaldehyde) terpolymer | 93.7% mild steel | 10−3 M in H2SO4 | 19 |
| Acrylic acid (AA), oxalic acid-allypolyethoxy carboxylate (APEM)-phosphorous acid (H3PO3) terpolymer | 79.77% carbon steel | 30 mg L−1 in 1 M HCl | 39 |
| Chitosan-acrylic acid-polysuccinimide terpolymer | 71.17% carbon steel | 500 mg L−1 in 3.5% NaCl | 40 |
| Acrylamide/styrene/maleic anhydride terpolymers (ASM) and thermally aged acrylamide/styrene/maleic anhydride terpolymers (A/ASM) | ASM (52%), A/ASM (94%)Mild steel | 3000 ppm in 3.5% NaCl | 41 |