Table 3.

The results of zeta potential and conductivity for different concentrations of Bzc and SDS.

Sample Weight (g/l) Concentration (ppm) Zeta potential (mV) Conductivity (mS/cm)
Bzc 0.2 200 43.6 0.178
Bzc 0.5 500 13 0.429
Bzc 1 1000 36.9 0.53
Bzc 1.5 1500 30 0.88
Bzc 2.5 2500 26.6 1.01
Bzc 3 3000 37.9 1.15
SDS 0.1 100 − 73.9 0.0614
SDS 0.2 200 − 43.4 0.083
SDS 0.4 400 − 69.3 0.13
SDS 0.6 600 − 69.5 0.214
SDS 1 1000 − 70.9 0.325