4. Values of Tension/Strain Tests, Carried Out at 25 °C for the PUCTS Composites in Different Compositions.
| sample | σ max/MPa | %/(ε) | E/MPa | displacement Δl/mm |
|---|---|---|---|---|
| PU | 0.69 | 14.4 | 0.04 | 1.60 |
| PU95CTS5 | 0.68 | 10.2 | 0.06 | 2.00 |
| PU90CTS10 | 0.83 | 6.89 | 0.12 | 1.10 |
| PU85CTS15 | 0.76 | 4.94 | 0.15 | 0.83 |
| PU75CTS25 | 0.73 | 3.81 | 0.19 | 0.61 |
| PU50CTS50 | 0.54 | 0.90 | 0.60 | 0.16 |