1. Comparison of Some Sulfide-Based Materials for CE Applications in DSSCs Measured at 100 mW/cm2 .
CE | electrolyte | active area (cm2) | Jsc(mA/cm2) | Voc (V) | FF | PCE (%) | ref. |
---|---|---|---|---|---|---|---|
CoS | I3 –/I– | 0.16 | 7.51 | 0.52 | 0.61 | 2.40 | |
NiS | I3 –/I– | 0.16 | 5.72 | 0.57 | 0.63 | 2.06 | |
ZnS | I3 –/I– | 0.16 | 5.39 | 0.46 | 0.45 | 1.12 | |
CoNi2S4 | I3 –/I– | 0.16 | 11.24 | 0.54 | 0.66 | 4.04 | |
Zn0.76Co0.24S | I3 –/I– | 0.16 | 10.49 | 0.55 | 0.61 | 3.52 | |
Zn0.76Co0.24S | I3 –/I– | N/R | 16.12 | 0.76 | 0.65 | 7.94 | |
MoS2 | I3 –/I– | N/R | 13.48 | 0.73 | 0.51 | 5.01 | |
MoS2/PEDOT | I3 –/I– | N/R | 13.73 | 0.74 | 0.69 | 7.00 | |
CuS | polysulfide | 0.2 | 16.34 | 0.64 | 0.38 | 3.83 | |
CuS-G | I3 –/I– | N/R | 10.33 | 0.71 | 0.66 | 4.83 | |
NSeC | I3 –/I– | N/R | 18.87 | 0.70 | 0.74 | 9.79 |
N/R: not reported.