Table 1. Electrospinning parameters for the chitosan/PEO solutions at increasing concentrations of glycerol.
| Glycerol concentration (%) | Voltage (kV) (needle; collector) | Feed rate (μL h−1) | Working distance (mm) |
|---|---|---|---|
| No glycerol | 26; −2 | 400 | 140 |
| 2% | 28; −3 | 300 | 125 |
| 5% | 27; −1.5 | 400 | 145 |
| 10% | 27; −2 | 500 | 135 |