Skip to main content
. 2025 Aug 22;15(36):29836–29863. doi: 10.1039/d5ra04739k

Fig. 13. Contour mapping of PCE (%) when ETL is (a) ZnO, (b) WS2, (c) WO3, (d) PCBM.