Skip to main content
. Author manuscript; available in PMC: 2025 Aug 25.
Published in final edited form as: ACS Sustain Chem Eng. 2025 Apr 22;13(17):6342–6354. doi: 10.1021/acssuschemeng.5c01330

Figure 2:

Figure 2:

(A) Overlay of GPC traces of 2-MeOPET-X polymers using HFIP as the eluent. The y-axis represents the normalized dRI detector response. (B) Overlay of DSC traces of 2-MeOPET-X polymers, second heating scan at 10 °C min−1. (C) Overlay of GPC traces of 2,6-MeOPET-X polymers using HFIP as the eluent. The y-axis represents the normalized dRI detector response. The shaded grey area represents the chromatograph past column resolution. (D) Overlay of DSC traces of 2,6-MeOPET-X polymers, second heating scan at 10 °C min−1.