Skip to main content
. 2025 Aug 7;7(16):10416–10429. doi: 10.1021/acsapm.5c01101

4. Mechanical Properties in Terms of Elastic Modulus (E), Tensile Strength at Break (σb), Eongation at Break (εb), and Toughness (T) of the Electrospun Pure PHBV, PHBV + Res, PHBV/ChCl:EG, PHBV/ChCl:EG + Res Biopapers.

biopaper E (MPa) σb (MPa) εb (%) toughness (mJ/m3)
pure PHBV 2512 ± 404 17.6 ± 0.7 1.9 ± 0.2 0.23 ± 0.05
PHBV + Res 3527 ± 572 34.7 ± 3.9 1.7 ± 0.2 0.33 ± 0.10
PHBV/ChCl:EG 3349 ± 406 38.9 ± 7.4 1.9 ± 0.3 0.45 ± 0.06
PHBV/ChCl:EG + Res 2694 ± 497 22.2 ± 0.9 1.6 ± 0.4 0.22 ± 0.05
a-b

Different letters in the same column indicate a significant difference among the samples (p < 0.05).