Skip to main content
. 2025 Oct 7;15:35011. doi: 10.1038/s41598-025-20119-1

Table 1.

The composition of the geopolymer paste mixes.

Mix code S SMA1 SMA3 SMA6 SSF1 SSF3 SSF6
Wt. % of slag (GGBFS) 100% 99% 97% 94% 99% 97% 94%
Wt.% of Moringa leaves ash (MLA) – 1% 3% 6% – – –
Wt.% of styrofoam (SF) – – – – 1% 3% 6%