. 2025 Dec 4;15(56):47790–47802. doi: 10.1039/d5ra07317k

Fig. 8. (a) Porosity evolution after formation cycling; (b) rate performances and (c) capacity retention at different current densities; charge–discharge profiles at 0.1–3.0 C for (d) graphite, (e) YNG-10%, (f) YNG-20%, (g) YNG-30%, (h) YNG-40%, and (i) YNG-50%.