Table 2. Results of the chemical investigations of the starting materials performed by ICP-OES and µ-XRF in p.p.m. by weight.
The results of the latter technique are shown in parentheses. Some of the ICP-OES values are below the limit of quantification (LOQ).
| Sample | Al | Ca | Ti | V | Cr | Mn | Fe | Zn |
|---|---|---|---|---|---|---|---|---|
| Arc-fusion grown material for initial feeds and seeds | 81 ± 0.8 | (313 ± 66) | < 4.8 (14 ± 3) | 36 ± 0.43 (25 ± 1) | 28 ± 0.67 (72 ± 18) | 13 ± 0.16 (4 ± 2) | 76 ± 0.88 (72 ± 2) | < 4.2 (0–15) |
| MgO ceramic target sample as delivered (manufactured by Kojundo, theoretical purity given by the manufacturer: 99.995%) | < 10.8 | (29 ± 1) | < 4.8 | < 9.3 | < 12.3 | 8 ± 0.07 | 8 ± 0.35 | 11 ± 0.1 |
| 5N (99.999%) MgO powder as delivered by Roth (Rotimetic) | < 3.1–16 | < 0.07–0.8 | < 0.8 | < 2 | < 1 | < 0.3 | < 1.9 | < 0.8 |