Table 2. Effect of crosslinking on the size of Ncs. All samples are prepared according to the general procedure using 5 wt% of EC in AcOEt (see also Table S1, Section S5 of the SI). A high-power ultrasound probe is used as the homogenizer.
| Entry | Cargo | Crosslinker | Avg. dimensionsa |
|---|---|---|---|
| 1 | Vanillin | — | 190 ± 45 nm |
| 2 | Vanillin | BTCA | 270 ± 96 nm |
| 3 | Vanillin | TMPG | 167 ± 35 nm |
| 4 | Vanillin | TMPG-BTCA | 217 ± 60 nm |
| 5 | — | TMPG-BTCA | 96 ± 40 nm |
| 6 | Vanillin | TMPG-TREN | 170 ± 40 nm |
| 7 | — | TMPG-BTCA + borax | 117 ± 40 nm |
Average dimensions of capsules are measured from SEM images (SI, Section 7.2) over a sample of 100 objects. Values are reported as mean ± standard deviation.