| Δa | Ductile crack extension |
| AIDE | Adsorption-induced dislocation emission |
| CT50 | Compact tension specimens with width W = 50 mm and thickness B = 25 mm |
| CTOA | Crack tip opening angle |
| EDM | Electric discharge machining |
| ESD | Equivalent spherical diameter |
| FEM | Finite element method |
| FIB | Focused ion beam |
| HE | Hydrogen embrittlement |
| HEDE | Hydrogen-enhanced decohesion |
| HELP | Hydrogen-enhanced localized plasticity |
| HESIV | Hydrogen-enhanced strain-induced vacancies |
| J | J-integral |
| MVC | Micro-void coalescence |
| PCHIP | Piecewise cubic Hermite interpolating polynomials |
| QC | Quasi-cleavage |
| ROI | Region of interest |
| SOD | Source-to-object distance |
| SEM | Scanning electron microscopy |
| SDD | Source-to-detector distance |
| SNR | Signal-to-noise ratio |
| µ-CT | Micro-computed tomography |