. 2026 Apr 22;18(20):10724–10735. doi: 10.1039/d6nr00524a

Fig. 3. (a) Custom-built cell setup for liquid gating of the mesoporous Ni–Co oxide coating prepared on top of the Si/Ti/Au substrate. (b) Schematic representation of the mesoporous structure of the Ni–Co oxide layer, illustrating the charge arrangement for a negatively biased sample. (c) Room-temperature magnetic hysteresis loops for as-annealed (green), gated (orange) and recovered (blue) states; (d) and (e) are the corresponding MS and HC values measured at each state.

Fig. 3