Table 2. Electrodeposition parameters applied to produce the Ni–Co films from the three baths.
| Parameters | Bath | ||
|---|---|---|---|
| 1 | 2 | 3 | |
| j (mA cm−2) | 40 | 40 | 40 |
| Time (s) | 60 | 170 | 30 |
| Stirring rate (rpm) | 300 | 100 | 100 |
| Bath temperature (°C) | 25 | 25 | 25 |
| pH | 2.3 | 2.3 | 2.3 |