Electroactive phase fraction (F(EA)), β phase fraction (F(β)), γ phase fraction (F(γ)) and overall β phase content taking into account the degree of crystallinity (Xβ) of all the pressed, stretched and electrospun samples

F(EA) F(β) F(γ) Xβ
Pressed PVDF 30 30 0 12
PVDF/PLA 95/05 28 28 0 12
PVDF/PLA 60/40 0 0 0 0
R3T60 PVDF 86 85 1 35
PVDFPLA 60/40 36 36 0 15
R3T80 PVDF 82 82 0 35
PVDF/PLA 95/05 81 81 0 33
R3T100 PVDF 71 71 0 35
PVDF/PLA 95/05 72 72 0 33
ES PVDF 87 58 29 30
PVDF/PLA 95/05 85 57 28 27