Table 2. BET surface area, pore volume, and pore size of ZnO and LaOCl/ZnO composite synthesized via the Terminalia catappa-assisted route.
| Material | S BET, m2 g−1 | Vpore, cm3 g−1 STP | d pore, nm |
|---|---|---|---|
| ZnO | 36.93 | 1.16 × 10−1 | 1.69 |