Table 4.

ΔTP00 values of the composite resins after 14 days of immersion in different teas

Composite Resin Distilled water Black tea Rooibos tea Peppermint tea
Estelite Palfique Paste −0.44 (−0.58—−0.17)A,b −4.08 (−5.13—−2.39)D,a −2.15 (−2.87—−1.69)C,a −0.69 (−1.00—−0.61)B,b
Estelite Posterior −0.13 (−0.26—−0.03)A,a −2.92 (−3.93—−2.63)C,a −2.00 (−2.15—−1.23)B,a −0.40 (−0.65—−0.06)A,a

*Values are presented as Median (Min–Max). Different uppercase letters within the same row indicate significant differences among tea groups for each composite resin (p <0.0083, Bonferroni−adjusted Mann–Whitney test). Different lowercase letters within the same column indicate significant differences between composite resins within the same tea group (p <0.0125, Bonferroni−adjusted Mann–Whitney test)