Table 2. Lateral crystallite size, defect spacing, and defect density of GO domains in GO–PVA–AgNW nanocomposites at different γ-irradiation doses.

γ Irradiation doses 0 kGy 250 kGy 500 kGy 1500 kGy
L a (nm) 22.21 18.51 18.45 19.25
L D (nm) 12.91 11.78 11.77 12.02
n D (×1011) 1.94 2.33 2.34 2.25