Skip to main content
. 2005 Jun 10;89(2):912–931. doi: 10.1529/biophysj.105.061150

TABLE 2.

Experimental values and parameter values

HaCaT
NHDF
Molecular Fibrillar Glass TCPS Molecular Fibrillar
v〉 (μm/h) 11 11 25 16 14 13
t0 (h) 3.1 1.8 2 3.6 1.1 1.1
vt0 (μm) 34 20 49 56 15 14
α (1/h) 1.7 1.6 2.2 1.9 2.3 1.8
β, respectively β0 (1/h) 4.7 4.8 1.5 2.1 6.8 3.5
β1 (1/μm) 0.043 0.073 0.015 0.057
γ (1/h) 1.0 1.3 1.6 0.8 0.8 0.7
σ0 (μm/h3/2) 11 14 33 25 24 21
σ1‖ (1/h1/2) 1.4 1.3 3.0 3.0 2.6 2.8
σ1⊥ (1/h1/2) 1.4 1.3 −0.02 0.006 0.29 −0.12

Values above the line are experimental values. Below the line are parameter values from fit of models to experimental data. HaCaT data obtained with 15-min time lapse; NHDF data with 30-min time lapse.