Skip to main content
. 2026 Aug 4;26:2147. doi: 10.1186/s12903-026-09524-8

Table 5.

Simple main effects of denture base within each reline material (Tukey-adjusted)

Reline material Comparison p
Ufi Gel Hard C Conventional vs. 3D-printed 0.001
Ufi Gel Hard C Conventional vs. Milled 0.086
Ufi Gel Hard C Milled vs. 3D-printed 0.206
Molloplast-B All base comparisons > 0.36 (ns)
GC Reline II Soft Conventional vs. 3D-printed < 0.001
GC Reline II Soft Milled vs. 3D-printed < 0.001
GC Reline II Soft Conventional vs. Milled 0.196

Within every base, the hard liner exceeded both soft liners (all p < 0.001)