Table 2.
Density of the ODN-probe 2 immobilized on the silicon surface (1.5 cm2 exposed area) as function of its concentration in solutiona
| ODN concentration in solution (µM) | ODN density on silicon surface (1012 strands/cm2) | Hybridization efficiency %b |
|---|---|---|
| 27.135 | 8.10 | 40 |
| 13.567 | 9.44 | 73 |
| 2.714 | 6.54 | 92 |
| 0.543 | 5.64 | 100 |
| 0.135 | 2.09 | 100 |
aReaction conditions: 4 ml phosphate buffer plus EDAC 0.026 M and NHS 0.0017 M; overnight; room temperature.
bAfter hybridization, denaturation and fluorescence measurements in solution (see text).