Skip to main content
. Author manuscript; available in PMC: 2006 May 18.
Published in final edited form as: Biomaterials. 2005 Aug 18;27(6):917–925. doi: 10.1016/j.biomaterials.2005.06.025

Fig. 5.

Fig. 5

Scanning electron microscopy images of the failed fracture surfaces of fatigue crack propagation specimens of cold irradiated and subsequently melted (CISM) UHMWPE at 25 (a, b, c), 50 (d, e, f), 75 (g, h, i), and 100 kGy (j, k, l).