Skip to main content
. 2006 Apr 14;91(1):217–226. doi: 10.1529/biophysj.106.081398

FIGURE 5.

FIGURE 5

(A) Force-indentation curves of a pore-spanning DODAB bilayer on pores with Rpore = 90 nm taken at different positions starting from the center (1) of the pore to the rim (4). (B) The average slope of more than 10 curves taken at each location as a function of the position ρ from the pore center (1) to the rim (4). The error bars originate from several independent force-indentation curves taken at the same spot.