Table 4.
Comparison of the ion activity product (IAP; mean ± standard deviation (SD)) and the thermodynamic stability* (ΔGo, mean ± SD) of the solutions containing the maximum concentrations of Ca and PO4 released from Zr-ACP/EBPADMA/TEGDMA/HEMA/MEP composites. Negative ΔGo value indicates solution supersaturated with respect to stoichiometric hydroxyapatite, Ca10(OH)2(PO4)6. Number of repetitive experiments in each group n ≥ 4.
Resin | IAP | ΔGo (kJ/mol) | ||
---|---|---|---|---|
unmilled ACP | milled ACP | unmilled ACP | milled ACP | |
ETHMI | 103.59 ± 0.76 | 106.63 ± 1.27 | − (4.35 ± 0.21) | − (3.42 ± 0.39) |
ETHMII | 102.51 ± 0.72 | 103.68 ± 1.19 | − (4.65 ± 0.22) | − (4.32 ± 0.36) |
ETHMIII | 102.05 ± 0.74 | 106.63 ± 0.68 | − (4.67 ± 0.23) | − (4.79 ± 0.20) |