Table 1.

Summary of flexural strength and healing efficacy for GFRP.

specimen description flexural strength (MPa) percent retained strength
control laminate—no damage 668±13 100
self-healing laminate—no damage 559±12 84
control laminate—damaged (2500 N peak load) 479±32 72
self-healing laminate—damaged, no repair 494±7 74
self-healing laminate—damaged +2 h at 100°C 578±28 87