Published in final edited form as: Biomaterials. 2008 Feb 11;29(14):2193–2202. doi: 10.1016/j.biomaterials.2008.01.006

Figure 9.

Figure 9

Magnetic resonance microscopy thick cross-sectional slice of hydrogel seeded with marrow stromal cell after14 days in osteogenic media (left portion) and the blank hydrogel (right portion). The internal diameter of the tube carrying the specimens above is 12.5 mm.