Skip to main content
. Author manuscript; available in PMC: 2009 Mar 10.
Published in final edited form as: Chem Phys Lett. 2008 Mar 10;454(1-3):85–90. doi: 10.1016/j.cplett.2008.01.075

Figure 3.

Figure 3

AFM images of samples: A –ITO/glass + Au particles; B – ITO/glass + Ag particles; C -ITO/glass + Au/Ag particles. X-Y dimensions for all scans are 5 x 5 μm.