Table 1.

Summary of polymer tuning parameter combinations.

Combination PEUU:collagen:elastin (%) Electrospinning Time (min) Final Concentration (%)
A 14.3:42.3:42.3 20 6
B 25:75:0 15 6
C 50:50:0 15 6
D 50:50:0 20 12